Title of article :
Preparation and characterization of BaSnO3 powders
by hydrothermal synthesis from tin oxide hydrate gel
Author/Authors :
Wensheng Lu، نويسنده , , Helmut Schmidt، نويسنده ,
Issue Information :
دوهفته نامه با شماره پیاپی سال 2007
Abstract :
BaSnO3 powders have been prepared from the
tin oxide hydrate gel and the Ba(OH)2 solution via
hydrothermal synthesis route. The influence of the process
parameters on the characteristics of BaSnO3 has been
studied. A powder with the single-phase of BaSnO3 can be
obtained only when the concentration of Ba(OH)2 solution
is no less than 0.2 M and the ratio of Ba:Sn lies between
1.0 and 1.2. At a hydrothermal temperature of 330 C or
higher, uniform BaSnO3 powders can be directly prepared
through hydrothermal reaction. When the hydrothermal
temperature is lower than 250 C, the as-prepared powder
consists of BaSn(OH)6 that transforms through an amorphous
phase into BaSnO3 by calcination at 260 C. In the
hydrothermal temperature range of 130–250 C, a higher
temperature can promote the crystallization of BaSnO3,
increases its specific surface area and decreases the average
particle size. The duration of the hydrothermal reaction
affects the morphology of the powder particles. The effects
of the nonaqueous solvents on the properties of powders
have also been investigated.