Pr and Nd substituted ´2:17´ magnets for elevated temperature application
Author :
Willman, C.J. ; Narasimhan, K. S V L
Author_Institution :
Crucible Research center, Pittsburgh, PA
Volume :
21
Issue :
5
fYear :
1985
fDate :
9/1/1985 12:00:00 AM
Firstpage :
1976
Lastpage :
1978
Abstract :
Results of Pr, Nd and (PrNd) substitution in the ´2:17´ type permanent magnet alloys are presented. Microstructural studies, crystal structure, anisotropy field (HA), Curie temperature (TC), and saturation magnetization (Ms) were used as tools for the evaluation of these alloys. Pr, Nd and (PrNd) increases Mswithout significantly affecting the Tc. HAdecreases when Sm is replaced by Pr, Nd or (PrNd). Several of the alloys investigated show promise to be permanent magnets.
Keywords :
Magnetic thermal factors; Permanent magnets; Anisotropic magnetoresistance; Heat treatment; Iron; Magnetic materials; Microstructure; Neodymium; Permanent magnets; Powders; Saturation magnetization; Temperature;
fLanguage :
English
Journal_Title :
Magnetics, IEEE Transactions on
Publisher :
ieee
ISSN :
0018-9464
Type :
jour
DOI :
10.1109/TMAG.1985.1064132
Filename :
1064132
Link To Document :
بازگشت