Abstract :
Results are presented from tests of the first full length prototype SSC dipole magnet. The cryogenic behavior of the magnet during a slow cooldown to 4.5K and a slow warmup to room temperature has been measured. Magnetic field quality was measured at currents up to 2000 A. Averaged over the body field all harmonics with the exception of b2and b8are at or within the tolerances specified by the SSC Central Design Group. (The values of b2and b8result from known design and construction defects which will be corrected in later magnets.) Using an NMR probe the average body field strength is measured to be 10.283 G/A with point to point variations on the order of one part in 1000. Data are presented on quench behavior of the magnet up to 3500 A (approximately 55% of full field) including longitudinal and transverse velocities for the first 250 msec of the quench.
Keywords :
Accelerator magnets, superconducting; Colliding-beam devices; Helium; Iron; Laboratories; Magnetic field measurement; Prototypes; Saturation magnetization; Steel; Superconducting coils; Superconducting magnets; Testing;