Abstract :
Rapidly quenched 4.5wt% silicon-iron ribbons 280/μm thick were cold-rolled with large thickness reduction in each rolling pass for a total thickness reduction of 70% or more. After annealing at high temperatures in a vacuum, they had highly oriented
Keywords :
Annealing; Core loss; Grain size; Temperature dependence;