• DocumentCode
    1075906
  • Title

    Performance Analysis of 60-nm Gate-Length III–V InGaAs HEMTs: Simulations Versus Experiments

  • Author

    Neophytou, Neophytos ; Rakshit, Titash ; Lundstrom, Mark S.

  • Author_Institution
    Network for Comput. Nanotechnol., Purdue Univ., West Lafayette, IN
  • Volume
    56
  • Issue
    7
  • fYear
    2009
  • fDate
    7/1/2009 12:00:00 AM
  • Firstpage
    1377
  • Lastpage
    1387
  • Abstract
    An analysis of recent experimental data for high-performance In0.7Ga0.3As high electron mobility transistors (HEMTs) for logic applications is presented. By using a fully quantum mechanical ballistic model, we simulate In0.7Ga0.3As HEMTs with gate lengths of LG = 60, 85, and 135 nm and compare the result to the measured IV characteristics, including drain-induced barrier lowering, subthreshold swing, and threshold voltage variation with gate insulator (wide-bandgap barrier layer) thickness, as well as on-current performance. To first order, devices with three different oxide thicknesses and channel lengths can all be described by a ballistic model for the channel with appropriate values of parasitic series resistance. For high gate and drain voltages ( VGS-VT=0.5 V and VDS=0.5 V), however, the ballistic simulations consistently overestimate the measured on-current (a sign of higher transconductance), and they do not show the experimentally observed decrease in on-current with increasing gate length. With no parasitic series resistance at all, the simulated on-current of the LG = 60 nm device is about twice the measured current. According to the simulation, the estimated ballistic carrier injection velocity for this device is about 2.7 times 107cm/s. Because of the importance of the semiconductor capacitance, the simulated gate capacitance is about 2.5 times less than the insulator/barrier capacitance. Possible causes of the transconductance degradation observed experimentally under high gate voltages in these devices are also explored. In addition to a possible gate-voltage-dependent scattering mechanism, the limited ability of the source to supply carriers to the channel and the effect of nonparabolicity are likely to play a role. The drop in the on-current at higher gate biases with increasing gate length, is an indication that the devices operate below th- e ballistic limit.
  • Keywords
    III-V semiconductors; ballistics; capacitance; gallium arsenide; high electron mobility transistors; indium compounds; semiconductor device models; semiconductor device testing; In0.7Ga0.3As; InGaAs; ballistic simulation; drain-induced barrier; gate-voltage-dependent scattering; high-electron mobility transistor; logical application; nonparabolicity effect; quantum mechanical ballistic model; semiconductor capacitance; simulated gate capacitance; size 135 nm; size 60 nm; size 85 nm; transconductance degradation; Analytical models; Capacitance; Electrical resistance measurement; HEMTs; Indium gallium arsenide; Insulation; Length measurement; MODFETs; Performance analysis; Voltage; Apparent; III–V; InAs; InGaAs; ballistic; high electron mobility transistor (HEMT); mobility; nonequilibrium Green´s function (NEGF); nonparabolicity; quantum; series resistance; source exhaustion; source starvation;
  • fLanguage
    English
  • Journal_Title
    Electron Devices, IEEE Transactions on
  • Publisher
    ieee
  • ISSN
    0018-9383
  • Type

    jour

  • DOI
    10.1109/TED.2009.2021437
  • Filename
    5075641