Abstract :
In this work, an improved version of a brittle fracture model, based on the formation of nitric acid in service through corona discharges, ozone, and moisture, is presented and is used to explain several different modes of brittle fracture. Similar to Part I, we refer throughout this article to the insulators as nonceramic insulators (NCIs). To prevent brittle fracture in-service, its causes must be first established. To prevent brittle fracture in-service, its causes must be first established.
Keywords :
brittle fracture; corona; failure analysis; insulators; brittle fracture model; brittle fracture prevention; corona discharges; failure analyses; failure prevention; nitric acid; nonceramic insulators; Corona; Corrosion; Failure analysis; Manufacturing processes; Moisture; Plastic insulation; Polymers; Stress; Surface cracks; Voltage;
fLanguage :
English
Journal_Title :
Electrical Insulation Magazine, IEEE
Publisher :
ieee
ISSN :
0883-7554
Type :
jour
DOI :
10.1109/MEI.2005.1489987
Filename :
1489987
Link To Document :
بازگشت