Title :
Annealing Temperature-Dependent Interfacial Behavior of Sequentially Plasma-Activated Silicon Bonded Wafers
Author :
Howlader, Matiar M R ; Zhang, Fangfang ; Kim, Moon.J.
Author_Institution :
Dept. of Electr. & Comput. Eng., McMaster Univ., Hamilton, ON, Canada
Abstract :
The annealing effects of voids, amorphous layer, and bonding strength in the sequentially plasma-activated silicon/silicon bonded interface were investigated. The interfacial silanol groups and water were condensed and removed, respectively, below and above annealing at 150°C. About 400°C, the bonding strength was reduced because of the increased void density associated with the plasma-induced surface defects and the increased thickness of interfacial silicon oxide. The increase of the interfacial thickness layer after annealing was confirmed by high-resolution transmission electron microscope and detected as silicon oxide using the electron energy loss spectroscopy. The surface roughness and contact angle were measured to explain the influence of plasma processing parameters on the interfacial behavior after annealing. While the water contact angle increased with the increase in the O2 reactive ion etching (RIE) time, the surface roughness was initially decreased and then increased. The surface activation with 400-W O2 RIE plasma induced defect sites such as nanopores and craters. This study indicates that the O2 RIE plasma time and power have to be as low as possible to reduce surface roughness and defects but have to be high enough to properly activate the surface with enough surface energy to achieve high quality of Si/Si interface.
Keywords :
annealing; bonding processes; contact angle; electron energy loss spectra; nanoporous materials; plasma materials processing; silicon; surface energy; surface roughness; transmission electron microscopy; voids (solid); Si-Si; amorphous layer; annealing; bonding strength; craters; electron energy loss spectroscopy; high-resolution transmission electron microscope; interfacial behavior; interfacial silanol groups; nanopores; plasma processing; plasma-induced surface defects; power 400 W; reactive ion etching; sequentially plasma-activated silicon bonded wafers; silicon oxide; surface energy; surface roughness; temperature 150 degC; void density; water contact angle; Annealing; electron energy loss spectroscopy (EELS); interfacial amorphous layer; sequentially plasma-activated bonding (SPAB); surface roughness; void density; water contact angle;
Journal_Title :
Microelectromechanical Systems, Journal of
DOI :