Title :
Effect of Fe, Cu, Zr and Ti on the magnetic properties of SmCo-1:7 magnets
Author :
Venkatesan, M. ; Rhen, Fernando M. F. ; Gunning, R. ; Coey, J.M.D.
Author_Institution :
Dept. of Phys., Trinity Coll., Dublin, Ireland
Abstract :
Summary form only given. Nanocrystalline Sm-Co-Cu-Ti magnets prepared by mechanical milling and subsequent annealing were reported to exhibit excellent room temperature coercivity. In this study, investigations of the effects of Fe, Cu, Zr and Ti substitution on magnetic properties of 1:7 magnets at temperatures up to 450/spl deg/C were investigated. The alloys with nominal composition SmCo/sub 6.6-x/(Fe/Zr)/sub x/Ti/sub 0.4/ (x = 0.0, 0.1 and 0.2) and SmCo/sub 6.8-x/Ti/sub x/Cu/sub 0.1/Fe/sub 0.1/ (x = 0.2, 0.3, 0.4) were prepared by arc melting in a high purity argon atmosphere. The alloy ingots were then crushed and milled for 12 h using high energy ball mill. The as-milled powders were annealed at 750/spl deg/C for 2 hours. X-ray diffraction confirms the formation of TbCu/sub 7/-type structure with minor amounts of the Tb/sub 2/Zn/sub 17/ rhombohedral phase. Grain size is /spl ap/ 40 nm. The authors show the room temperature hysteresis loops of ball-milled SmCo-1:7 compositions with Fe and Zr doping. All compounds exhibit room temperature coercivity of more than 1 T. Substitution of Zr and Ti increases the room temperature coercivity whereas Fe substitution leads to an decrease of the magnetization but a decrease of the coercivity. A room temperature intrinsic coercivity of around 2.5 T is obtained for compositions SmCo/sub 6.4/Zr/sub 0.2/Ti/sub 0.4/ and SmCo/sub 6.4/Fe/sub 0.1/Zr/sub 0.1/Ti/sub 0.4/.
Keywords :
X-ray diffraction; alloying additions; annealing; cobalt alloys; coercive force; copper alloys; ferromagnetic materials; grain size; iron alloys; mechanical alloying; nanostructured materials; permanent magnets; powder technology; samarium alloys; titanium alloys; zirconium alloys; 12 h; 2 h; 40 nm; 450 degC; 750 degC; SmCo/sub 6.4/Fe/sub 0.1/Zr/sub 0.1/Ti/sub 0.4/; SmCo/sub 6.4/Zr/sub 0.2/Ti/sub 0.4/; SmCo/sub 6.6-x/(Fe/Zr)/sub x/Ti/sub 0.4/; SmCo/sub 6.6-x/(FeZr)/sub x/Ti/sub 0.4/; SmCo/sub 6.8-x/Ti/sub x/Cu/sub 0.1/Fe/sub 0.1/; X-ray diffraction; annealing; arc melting; grain size; mechanical milling; nanocrystalline Sm-Co-Cu-Ti magnets; room temperature coercivity; Annealing; Coercive force; Copper alloys; Iron alloys; Magnetic properties; Magnets; Milling; Temperature; Titanium alloys; Zirconium;
Conference_Titel :
Magnetics Conference, 2002. INTERMAG Europe 2002. Digest of Technical Papers. 2002 IEEE International
Conference_Location :
Amsterdam, The Netherlands
Print_ISBN :
0-7803-7365-0
DOI :
10.1109/INTMAG.2002.1000704