Abstract :
In this paper, the effect of AC Corona on the hydrophobicity of room temperature vulcanizing (RTV) silicone rubber materials is studied with a pin-plate electrode corona accelerate aging model. Experiments show that AC corona can make the RTV specimen hydrophobicity lose rapidly, further, the hydrophobicity recovery character of RTV specimen is also researched through a long time of corona test, as a result, it is found that the RTV specimen hydrophobicity recovery speed is not continuous, but having an alternate process of "speed up" and "slow down". After corona time reaches a certain time, the hydrophobicity recovery time dramatically becomes longer but it still can not fully restore to the initial value in the end. meanwhile research find that when the corona time is in a certain range, after the hydrophobicity recovery, the final static contact angle is much larger than the initial value before the corona.
Keywords :
corona; hydrophobicity; silicone rubber insulators; AC corona; RTV silicone rubber hydrophobicity loss; aging model; pin-plate electrode corona; room temperature vulcanizing rubber materials; Chemicals; Corona; Discharges; Materials; Rubber; Surface discharges; Surface treatment; Aging; RTV (room temperature vulcanizing) silicone rubber; corona; hydrophobicity; static contact angle;
fLanguage :
English
Publisher :
ieee
Conference_Titel :
Electrical and Control Engineering (ICECE), 2011 International Conference on
Conference_Location :
Yichang
Print_ISBN :
978-1-4244-8162-0
Type :
conf
DOI :
10.1109/ICECENG.2011.6057582
Filename :
6057582
Link To Document :
بازگشت