• DocumentCode
    2021737
  • Title

    Fracture strength of silicon wafer after different wafer treatment methods

  • Author

    Zhou, Linfeng ; Qin, Fei ; Sun, Jinglong ; Chen, Pei ; Yu, Huiping ; Wang, Zhongkang ; Tang, Liang

  • Author_Institution
    College of Mechanical Engineering and Applied Electronics Technology, Beijing University of Technology, China
  • fYear
    2015
  • fDate
    11-14 Aug. 2015
  • Firstpage
    871
  • Lastpage
    874
  • Abstract
    With the increase of wafer diameter and the reduction of wafer thickness, the fracture strength of silicon wafer decreases dramatically, which has drawn much more attention in recent years. Three-point bending test is a frequently cited method used to measure the fracture strength of silicon wafer, and the measured strength is sensitive to the edge defect caused by dicing. This paper proposes a grinding and polishing wafer treatment method to eliminate the defect along the sample edges. And the fracture strength of the treated and the untreated samples are compared in this study. The result shows that the fracture strength of the treated samples is much higher than those of the untreated.
  • Keywords
    Coolants; Silicon; Surface treatment; Wheels; fracture strength; silicon wafer; three-point bending test;
  • fLanguage
    English
  • Publisher
    ieee
  • Conference_Titel
    Electronic Packaging Technology (ICEPT), 2015 16th International Conference on
  • Conference_Location
    Changsha, China
  • Type

    conf

  • DOI
    10.1109/ICEPT.2015.7236718
  • Filename
    7236718