    Dielectric properties of ethylene-propylene rubber in cryogenic temperature region

  • Author

    Mizuno, Yukio ; Mitsuyama, Yasuichi ; Nagao, Masayuki ; Kosaki, Masamitsu

  • Author_Institution
    Nagoya Inst. of Technol., Japan
  • Volume
    2
  • fYear
    1994
  • fDate
    3-8 Jul 1994
  • Firstpage
    475
  • Abstract
    The effect of additives such as crosslinking agent and fillers on tan δ of ethylene-propylene rubber (EPR) was examined at temperatures between 4.2 K and 300 K. Thickness dependence of tan δ was also evaluated by using EPR films of different thickness and an extruded EPR insulated cable sample. The results show that additives increase tan δ of relatively thin EPR films even in cryogenic temperature region, whereas the thicker samples practical to cable insulation do not give intolerable dielectric loss. The remedy to tan δ increase due to the polymer contraction relative to shielding wires has been established
  • Keywords
    dielectric loss measurement; dielectric losses; ethylene-propylene rubber; insulation testing; low-temperature techniques; power cable insulation; 4.2 to 300 K; EPR films; additive effects; crosslinking agent; cryogenic temperature region; dielectric properties; ethylene-propylene rubber; extruded EPR insulated cable; fillers; polymer contraction; power cables; shielding wires; tan δ; thickness dependence; Additives; Cable insulation; Cable shielding; Cryogenics; Dielectric losses; Dielectrics and electrical insulation; Paramagnetic resonance; Rubber; Superconducting cables; Temperature dependence;
  • fLanguage
    English
  • Publisher
    ieee
  • Conference_Titel
    Properties and Applications of Dielectric Materials, 1994., Proceedings of the 4th International Conference on
  • Conference_Location
    Brisbane, Qld.
  • Print_ISBN
    0-7803-1307-0
  • Type

    conf

  • DOI
    10.1109/ICPADM.1994.414050
  • Filename
    414050