DocumentCode :
2190499
Title :
Direct evidence for multiple vibrational excitation of Si-H/D bonds for hot-carrier degradation of MOS transistors
Author :
Zhi Chen ; Pangleen Ong
Author_Institution :
Dept. of Electr. & Comput. Eng., Kentucky Univ., Lexington, KY, USA
fYear :
2002
fDate :
24-26 June 2002
Firstpage :
189
Lastpage :
190
Abstract :
The study of the desorption of hydrogen (H) and deuterium (D) on silicon in ultra high vacuum (UHV) by scanning tunneling microscopy (STM) led to the discovery of the giant H/D isotope effect. It was later used in passivation of the SiO/sub 2//Si interface, leading to large improvement of the hot-carrier lifetime of MOS transistors (J.W. Lyding et al, Appl. Phys. Lett., vol. 68, p. 2526, 1996). It is known that desorption mechanisms for the Si-H/D bonds by STM are multiple vibrational excitation at low voltage (T.-C. Shen et al, Science vol. 268, p. 1590, 1995). However, the chemical environment of the SiO/sub 2//Si interface in MOS devices is very different from that of Si in UHV, because in MOS transistors, electrons not only directly excite the Si-H/D bonds, but also are injected into the oxide. Recently, we showed that electrons that are injected into the oxide may not break Si-H/D bonds and only electrons that remain in the channel (and do not overcome the oxide/Si barrier) break the Si-H/D bonds (Z. Chen et al, IEEE Electron Dev. Lett. vol. 21, p. 24, 2000). Although it was suggested that the mechanisms for breakage of Si-H/D bonds in MOS transistors should be analogous to the explanation for the STM experiments, there is no direct experimental evidence to support the suggestion. In this paper, we present experimental results to show that the quantitative H/D isotope effect is dependent on the channel current density, which support the multiple vibrational excitation mechanisms.
Keywords :
MOSFET; bonds (chemical); deuterium; hot carriers; hydrogen; semiconductor device reliability; semiconductor device testing; silicon; vibrational states; MOS devices; MOS transistors; STM; Si-D; Si-H; Si-H/D bond breakage mechanisms; Si-H/D bonds; Si-SiO/sub 2/; SiO/sub 2//Si interface; channel current density; channel electrons; chemical environment; deuterium desorption; hot-carrier degradation; hot-carrier lifetime; hydrogen desorption; multiple vibrational excitation; oxide electron injection; passivation; quantitative H/D isotope effect; scanning tunneling microscopy; ultra high vacuum; Degradation; Deuterium; Electrons; Hot carriers; Hydrogen; Isotopes; MOSFETs; Microscopy; Silicon; Tunneling;
fLanguage :
English
Publisher :
ieee
Conference_Titel :
Device Research Conference, 2002. 60th DRC. Conference Digest
Conference_Location :
Santa Barbara, CA, USA
Print_ISBN :
0-7803-7317-0
Type :
conf
DOI :
10.1109/DRC.2002.1029593
Filename :
1029593
Link To Document :
بازگشت