    Fabrication of textured Bi4Ti3O12 by templated grain growth

  • Author

    Horn, J.A. ; Zhang, S.C. ; Selvaraj, U. ; Messing, G.L. ; Trolier-McKinstry, S. ; Yokoyama, M.

  • Author_Institution
    Pennsylvania State Univ., University Park, PA, USA
  • Volume
    2
  • fYear
    1996
  • fDate
    18-21 Aug 1996
  • Firstpage
    943
  • Abstract
    Dense, textured Bi4Ti3O12 was produced by templated grain growth (TGG). Phase pure nanosized Bi4 Ti3O12 powder was prepared by coprecipitation of an aqueous solution of Bi2O3 and TiO(OH)Cl. Plate-like particles with aspect ratios of 6-60 were obtained by the molten salt method at 1100°C. The plate-like particles were dispersed in the calcined powder and oriented by tape casting and laminating. The laminates were sintered from 900-1100°C to obtained textured ceramics up to 96% dense. Texture development was investigated by X-ray diffraction, and dielectric measurements were made on both templated and untemplated samples
  • Keywords
    bismuth compounds; ceramics; ferroelectric materials; grain growth; laminates; nanostructured materials; powder technology; precipitation (physical chemistry); sintering; texture; 900 to 1100 C; Bi4Ti3O12; X-ray diffraction; aspect ratio; calcination; coprecipitation; dielectric measurement; dispersion; fabrication; laminate; molten salt method; nanosized powder; plate-like particles; tape casting; templated grain growth; textured ceramic; Bismuth; Ceramics; Dielectric measurements; Fabrication; Ferroelectric materials; Laminates; Powders; Tape casting; Titanium compounds; X-ray diffraction;
  • fLanguage
    English
  • Publisher
    ieee
  • Conference_Titel
    Applications of Ferroelectrics, 1996. ISAF '96., Proceedings of the Tenth IEEE International Symposium on
  • Conference_Location
    East Brunswick, NJ
  • Print_ISBN
    0-7803-3355-1
  • Type

    conf

  • DOI
    10.1109/ISAF.1996.598182
  • Filename
    598182