Title :
Corrosion Analysis for Co-Ni-O Film Adopted as the Magnetic Layer of Metal Evaporated Tape
Author :
Nouchi, N. ; Kai, Y. ; Maesawa, Y. ; Nakamura, N. ; Shinohara, K.
Author_Institution :
Matsushita Electric Industrial Co., Ltd.
Volume :
6
Issue :
4
fYear :
1991
fDate :
4/1/1991 12:00:00 AM
Firstpage :
274
Lastpage :
283
Abstract :
Corrosion in Co-Ni-O film, which is adopted as the magnetic layer in metal evaporated tape media, was examined through aging tests, measurements of anode polarized characteristics, and analysis of both chemical bonding by ESCA and of crystallographic characteristics by RHEED. The following results were obtained. 1) The experimental results for exposure tests were strongly correlated with the anode characteristics. 2) Corrosion occurring in the uppermost layer of Co-Ni-O film exposed to high temperatures and high humidity progressed as follows: CoO+H2O¿Co (OH)2, 2Co (OH)2+0.5O2¿2CoOOH+H2O. 3) Both oxygen gas introduced in the deposition process, and fluorine lubricant coated onto the surface of the Co-Ni-O film give effective protection against corrosion.
Keywords :
Aging; Anodes; Bonding; Chemical analysis; Corrosion; Crystallography; Magnetic analysis; Magnetic films; Polarization; Testing;
fLanguage :
English
Journal_Title :
Magnetics in Japan, IEEE Translation Journal on
Publisher :
ieee
ISSN :
0882-4959
Type :
jour
DOI :
10.1109/TJMJ.1991.4565151
Filename :
4565151
Link To Document :
بازگشت