The Effects of Moisture on the Breakdown - Pulse - Noise of Mineral - Insulated Instrument Cable
Author :
Hardtke, F.C.
Author_Institution :
University of Missouri Rolla, Mo. 65401
Volume :
22
Issue :
1
fYear :
1975
Firstpage :
681
Lastpage :
685
Abstract :
Cable resistances (R) and breakdown-pulse-noise (BPN) were measured before, during, and after heating 60-cm portions of a 10-meter mineral-insulated coaxial cable to various temperatures (T), mostly 320°C. A severe BPN-condition and a very low R within about 60 cm of the high-T end of the cable was shown to be due to atmospheric moisture admitted through an end-seal leak inflicted by a previous test. A similar, but much less severe, BPN-condition 90 to 120 cm removed from either end was attributed to a small amount of moisture that had collected at these positions during the same previous test independent of the end-seal leak. These results suggest that the BPN problem might be eliminated by better hygroscopic measures in cable manufacture.
Keywords :
Atmospheric measurements; Cable insulation; Coaxial cables; Electric breakdown; Electrical resistance measurement; Instruments; Minerals; Moisture; Resistance heating; Testing;
fLanguage :
English
Journal_Title :
Nuclear Science, IEEE Transactions on
Publisher :
ieee
ISSN :
0018-9499
Type :
jour
DOI :
10.1109/TNS.1975.4327728
Filename :
4327728
Link To Document :
بازگشت