  • Abstract
    The dielectric loss tangent of yttria stabilised zirconia (YSZ) was measured at approximately 5.5 GHz using the dielectric rod resonator method (DRRM). The measured values of tan delta were 9*10-4 at 300 K and 3*10-4 at 77 K.
  • Keywords
    ceramics; dielectric losses; yttrium compounds; zirconium compounds; 300 K; 5.6 GHz; 77 K; Y 2O 3ZrO 2; dielectric loss tangent; dielectric rod resonator method;