On the dependence of intrinsic coercivity on grain size in the nucleation-controlled rare earth-iron-boron sintered magnets
Author :
Hirosawa, Satoshi
Author_Institution :
Sumitomo Special Metals Co. Ltd., Osaka, Japan
Volume :
25
Issue :
5
fYear :
1989
fDate :
9/1/1989 12:00:00 AM
Firstpage :
3437
Lastpage :
3439
Abstract :
The temperature dependence of the intrinsic coercivity of Pr-Fe-B sintered magnets with closely packed and isolated grains of various sizes has been measured. It was found that the reduction factor of the nucleation field in comparison to the ideal value (HA) is affected by grain size alterations, while the local demagnetization coefficient remains constant. The result is discussed in terms of intra- and intergranular magnetic correlations. A change in the intergranular correlation length is suggested to be one of possible causes of the observed dependence of the reduction factor on the grain size
Keywords :
boron alloys; coercive force; demagnetisation; ferromagnetic properties of substances; grain size; iron alloys; permanent magnets; praseodymium alloys; sintering; PrFeB sintered magnets; grain size; intergranular correlation length; intergranular magnetic correlations; intragranular magnetic correlations; intrinsic coercivity; local demagnetization coefficient; nucleation field; permanent magnets; temperature dependence; Boron alloys; Coercive force; Grain size; Human computer interaction; Iron alloys; Magnetic anisotropy; Magnetic field measurement; Magnets; Size measurement; Temperature dependence;
fLanguage :
English
Journal_Title :
Magnetics, IEEE Transactions on
Publisher :
ieee
ISSN :
0018-9464
Type :
jour
DOI :
10.1109/20.42327
Filename :
42327
Link To Document :
بازگشت