Abstract
The most common and maximum radii of craters on cathodes of copper, mild steel, silver, silver cadmium oxide and aluminium having various oxide film thicknesses, are reported following 4.5 A arcing of duration between 3.8 ns and 3.5 ¿¿s. The increase in crater radius with arc duration is examined in the light of a simple joule-heating model in a hemispherical region from which material is lost to form a crater. All the results except one conform with adiabatic joule heating, the one exception involving heat conduction into the cathode being no longer negligible. A brief comparison with cratering in cathodes of vacuum arcs is made, showing that these are of the latter type where joule heating provides the dominant energy input and the crater radius tends to increase to a value where this input is balanced by thermal conduction into the bulk metal. Close agreement with the model confirms earlier estimates by other methods of mean emitting site currents, current densities and lifetimes for copper and steel, and then enables these quantities to be estimated for the first time for silver, silver cadmium oxide, aluminium and also for mild steel with a relatively thick oxide film.
Keywords
arcs (electric); oxide coated cathodes; 4.5 A arcing; Ag; AgCdO; Al; Cu; cathodes; emitting sites; joule heating; mild steel; nonrefractory arc cathodes; oxide film thicknesses; radii of craters; thermal conduction;
fLanguage
English
Journal_Title
Physical Science, Measurement and Instrumentation, Management and Education - Reviews, IEE Proceedings A
Publisher
iet
ISSN
0143-702X
Type
jour
DOI
10.1049/ip-a-1.1980.0067
Filename
4644759
Link To Document