  • Abstract
    The deformation of the supporting tube during the c.v.d. process for optical fibre fabrication is completely suppressed by controlling the internal pressure of the tube. A 14 km length single-mode fibre with attenuation loss of about 3.2 dB/km at 0.85 ¿m was fabricated by this improved method.
  • Keywords
    chemical vapour deposition; optical fibres; optical workshop techniques; 14 km single mode optical fibre; 3.2 dB/km attenuation; chemical vapour deposition; long optical fibres; optical fibre fabrication; supporting tube deformation suppression;
  • fLanguage
    English
  • Journal_Title
    Electronics Letters
  • Publisher
    iet
  • ISSN
    0013-5194
  • Type

    jour

  • DOI
    10.1049/el:19780060
  • Filename
    4240844