Abstract
The magnetic properties of Sm2(Co,Fe,Cu,Zr)17 magnets were improved by increasing the Fe content without raising the Zr content. With increasing Fe content, the remanence rises monotonically while the intrinsic coercive force drops sharply for 0.27<v <0.29 and then increases for 0.30<v <0.33 in Sm(CobalFevCu0.056Zr0.02) 7.546. For the nominal composition Sm(Co0.612Fe 0.316Cu0.052Zr0.02)7.73, most magnets developed (BH)max=31-33 MGOe while some reached 33-34 MGOe. Still higher Fe contents may result in further improvement of Sm2TM17 magnets
Keywords
cobalt alloys; coercive force; copper alloys; ferromagnetic properties of substances; iron alloys; permanent magnets; remanence; samarium alloys; zirconium alloys; Fe content; Sm-Co-Fe-Cu-Zr; Sm2(Co,Fe,Cu,Zr)17; intrinsic coercive force; magnetic properties; maximum energy products; remanence; Coercive force; Iron; Magnetic materials; Magnetic properties; Magnets; Samarium; Solids; Sun; Temperature; Zirconium;
fLanguage
English
Journal_Title
Magnetics, IEEE Transactions on
Publisher
ieee
ISSN
0018-9464
Type
jour
DOI
10.1109/20.42433
Filename
42433
Link To Document