Abstract :
A variety of epoxy resins, filler mixtures, and adhesion additives were examined in semiconductor molding compounds for solder-reflow crack resistance (popcorn crack resistance). A limited comparison of molding compound high temperature strength properties and extent of popcorn cracking suggests no strong positive correlation. On the other hand, factors that might have an impact on adhesive properties of the molding compound, such as Low melt viscosity resins and putative adhesion additives appear to have the greatest impact. A molding compound developed with these factors showed no internal or external cracks on 84 Lead QFP´s (29.2×29.2×3.68 mm) after 72 h of 85°C/85% R.H. and one 10-s solder dip at 260°C. Nor were any external cracks observed after 168 h of 85°C/85% R.H. and one solder dip. However, minor internal cracks were observed
Keywords :
adhesion; cracks; integrated circuit packaging; reflow soldering; semiconductor device packaging; surface mount technology; thermal stress cracking; QFP; adhesion additives; adhesive properties; epoxy resins; filler mixtures; high temperature strength properties; low melt viscosity resins; popcorn crack resistance; semiconductor molding compounds; solder-reflow crack resistant compound; Additives; Adhesives; Epoxy resins; Immune system; Lead; Moisture; Packaging; Silicon compounds; Temperature; Viscosity;
fLanguage :
English
Journal_Title :
Components, Packaging, and Manufacturing Technology, Part A, IEEE Transactions on
Publisher :
ieee
ISSN :
1070-9886
Type :
jour
DOI :
10.1109/95.465164
Filename :
465164
Link To Document :
بازگشت