    Germanium-oxide glass optical fibre prepared by VAD method

  • Author

    Takahashi, Hiroki ; Sugimoto, Ichiro ; Sato, Takao

  • Author_Institution
    Furukawa Electric Co. Ltd., Central Research Laboratory, Tokyo, Japan
  • Volume
    18
  • Issue
    10
  • fYear
    1982
  • Firstpage
    398
  • Lastpage
    399
  • Abstract
    Germanium-oxide glass optical fibre doped with antimony for transmission of the 2 to 3 ¿m band has been prepared by the vapour-phase axial deposition (VAD) method. An attenuation loss of 13 dB/km at 2.05 ¿m and 70 dB/km at 2.4 ¿m has been achieved.
  • Keywords
    antimony; germanium compounds; glass fibres; optical fibres; vapour deposition; GeO2:Sb glass optical fibre; attenuation loss; vapour-phase axial deposition;