Improved formulas are obtained to provide more accurate determination of magnetic bubble material parameters such as material length

and saturation magnetization

based on the measurements of domain stripe width and bubble collapse field. The improvement takes into consideration the effects of finite uniaxial anisotropy parameter

in the formulas. These improved formulas are based on the numerical results obtained from micromagnetic domain calculations of periodic stripes and of an isolated axisymmetric bubble.