  • Abstract
    A low-OH-content and long-length optical fibre has been made by the v.a.d. method. The OH content in the rod preform was reduced to about 0.4 p.p.m. utilising the chemical reactions of SOCl2 or CCl4 with OH ions and H2O molecules In the porous glass rod. The minimum loss of the fibre, 20km long, was 1.0±0.1 dB/km at 1.2¿m.
  • Keywords
    chemical vapour deposition; optical fibres; optical glass; optical workshop techniques; loss spectrum; low OH content optical fibre; rod preform IR transmission spectrum; vapour phase axial deposition method;
  • fLanguage
    English
  • Journal_Title
    Electronics Letters
  • Publisher
    iet
  • ISSN
    0013-5194
  • Type

    jour

  • DOI
    10.1049/el:19780362
  • Filename
    4249524