Title of article :
Mechanical failure of anodized film of aluminium in bending
Author/Authors :
W. Bensalah، نويسنده , , K. Elleuch، نويسنده , , M. Feki، نويسنده , , M. De Petris-Wery، نويسنده , , H.F. Ayedi، نويسنده ,
Issue Information :
ماهنامه با شماره پیاپی سال 2009
Pages :
9
From page :
3141
To page :
3149
Abstract :
The mechanical properties of electrolytic oxide layers elaborated on aluminium substrate in oxalic–sulphuric acid bath were optimized using a four variables doehlert experimental design (bath temperature, anodic current density, sulphuric acid and oxalic acid concentrations). Thickness measurements and flexural tests were conducted. A sudden decrease of the load, indicative of film failure, was observed upon the load–deflection curve. The deflection at failure and the maximum load for each layer were deduced from the corresponding load–deflection curve. The isoresponse curves study and the optimum path study of the three retained responses: thickness, maximum load and deflection at failure, showed that the experimental conditions, where the three optima were found, were opposite. In order to maximize in the same time the three responses, multicriteria optimization using the desirability function was achieved. In so doing, the determined optimal anodizing conditions were: Cox = 13.6 g L−1, T = 21.4 °C, j = 2.48A dm−2, Csul = 186.3 g L−1, while the corresponding estimated response values were 57.6 μm, 775 N and 4.16 mm for thickness, maximum load and deflection at failure, respectively.
Keywords :
Flexural response , Aluminium anodizing , Doehlert design
Journal title :
Materials and Design
Serial Year :
2009
Journal title :
Materials and Design
Record number :
1068371
Link To Document :
بازگشت