Abstract :
A new kind of aromatic diamine monomer containing pyridine unit, 2,6-bis(4-aminophenoxy-4′-benzoyl)pyridine (BABP), was synthesized successfully. The Friedel–Crafts acylation of phenyl ethyl ether with 2,6-pyridinedicarbonyl chloride formed 2,6-bis(4,4′-dihydroxybenzoyl)-pyridine (BHBP), BHBP was changed into 2,6-bis(4-nitrophenoxy-4′-benzoyl)-pyridine (BNBP) by the nucleophilic substitution reaction of it and p-chloronitrobenzene, and BNBP was reduced with SnCl2 and HCl in ethanol to form the diamine monomer BABP finally, the diamine monomer BABP could be obtained in quantitative yield. A series of novel polyimides were prepared by polycondensation of BABP with various aromatic dianhydrides in N-methy-2-pyrrolidone (NMP) via the conventional two-step method. Experimental results indicated that some of the polyimides were soluble both in strong dipolar solvents (N-methy-2-pyrrolidone or N,N-dimethylacetamide) and in common organic solvents tetrahydrofuran. The resulting polyimides showed exceptional thermal and thermooxidative stability, no weight loss was detected before a temperature of 450 °C in nitrogen, and the values of glass-transition temperature of them were in the range of 208–324 °C. Wide-angle X-ray diffraction measurements revealed that these polyimides were predominantly amorphous.
Keywords :
Thermostablity , Synthesis , Pyridine-containing polyimides