Title of article :
Creep failure of cracking heater at a petrochemical plant
Author/Authors :
El-Batahgy، نويسنده , , Mohamed A. and Zaghloul، نويسنده , , B.، نويسنده ,
Issue Information :
روزنامه با شماره پیاپی سال 2005
Pages :
7
From page :
239
To page :
245
Abstract :
After two and half years of operation, a bend tube in a cracking heater at an ethylene plant failed due to creep cracking. Creep damage occurred as a result of metallurgical instability including coarsening of carbides that caused softening and initiation of voids or wedge-type intergranular cracks. This was accelerated due to increasing inner surface temperature during decoking process. Thermal fatigue contributed to the failure as a result of temperature variations due to several shutdown–startup operations. imize such failure in futures, periodic inspection to monitor crack formation was scheduled. Nondestructive tests including dye penetrant test for surface cracking and radiographic test for internal crack were implemented.
Keywords :
Nickel-base superalloy , Weld quality , creep damage , Thermal fatigue , Periodic inspection
Journal title :
Materials Characterization
Serial Year :
2005
Journal title :
Materials Characterization
Record number :
2266148
Link To Document :
بازگشت