Abstract- Optimum conditions for fabrication of vertically aligned carbon nanotubes (CNT) and
alumina nanocomposite have been investigated in this research. Porous anodic aluminum oxide
(AAO) was synthesized using Oxalic acid (0.3 M) under two voltages of 40 and 60. In order to
synthesize CNT/AAO nanocomposites, carbon nanotubes were grew in a chemical vapor deposition
(CVD) reactor using acetylene (C2H2) and argon (Ar) as carbon source and carrier gas,
respectively. In the experimental study, temperature of CVD reactor and C2H2/Ar flow ratio were
changed in the range of 550oC-750oC and 0.005-0.05, respectively. The results showed that when the
temperature of CVD reactor is set to 650oC and C2H2/Ar flow ratio is equal to 0.01, vertically
aligned CNTs with appropriate structures are obtained. It is also found that CNT/AAO
nanocomposites fabricated in 40 (V) has tubular structure while Y-branched structured is obtained
when 60 (V) is used.