Abstract :
A study of polyethylene terephthalate (PET) and polypropylene (PP) treated by corona discharge for a short time is presented. Different techniques of analysis such as inverse chromatography, infrared spectroscopy, loss tangent and electric strength were used. Working at 50 Hz with a gap of 2 mm and different gases, the analysis of the polymer after treatment has shown that a limit in the transformation of the surface may be considered. Thus a critical time is defined between a pure transformation and a degradation. This latter phase is also studied with a cross linked polyethylene (XLPE). The infrared analysis and electric strength measurements have shown the role played by the relative humidity present in air.
Keywords :
Corona; Degradation; Dielectric materials; Electric variables measurement; Gases; Infrared spectra; Polyethylene; Polymers; Positron emission tomography; Surface treatment;
fLanguage :
English
Journal_Title :
Electrical Insulation, IEEE Transactions on
Publisher :
ieee
ISSN :
0018-9367
Type :
jour
DOI :
10.1109/TEI.1982.298550
Filename :
4080935
Link To Document :
بازگشت