Title :
High kt piezoelectric ceramics
Author :
Wu, L. ; Liang, C.K. ; Lu, Y.G.
Author_Institution :
Dept. of Electr. Eng., Nat. Cheng Kung Univ., Tainan, Taiwan
Abstract :
The properties of modified lead titanate ceramics (Pb,La) (Ti,Mn)O 3 doped with Cr2O3 are investigated. The dielectric constant increases with increasing addition of Cr2 O3, and the fundamental thickness coupling factor k t does not show a large fluctuation. But the planar coupling factor shows a lower value for 0.4-0.8 wt.% additives. Meanwhile, at about 0.4 wt.% doping, the coupling factor kt and the temperature coefficient of the third overtone thickness extension vibration mode have improved values of 0.3 and -6 p.p.m./°C, respectively. Thus the chromium addition may be considered as a promoter of stabilization in a certain range. The pure third overtone spectrum of the thickness mode can be strengthened by decreasing the electrode diameter, and the frequency constant reaches about 6820 kHz-mm
Keywords :
ceramics; chromium compounds; lanthanum compounds; lead compounds; permittivity; piezoelectric materials; piezoelectric oscillations; PbLaTiO3MnO3:Cr2O3; dielectric constant; electrode diameter; frequency constant; piezoelectric ceramics; planar coupling factor; stabilization; temperature coefficient; thickness coupling factor; third overtone thickness extension vibration mode; Ceramics; Chromium; Dielectric constant; Doping; Electrodes; Fluctuations; Frequency; Lead; Temperature; Titanium compounds;
Conference_Titel :
Ultrasonics Symposium, 1990. Proceedings., IEEE 1990
Conference_Location :
Honolulu, HI
DOI :
10.1109/ULTSYM.1990.171459