Abstract :
By means of breaking tests on different Ni content for AgNi contact materials in a CKS contact material machine, an attempt was made to elucidate the formation mechanisms of the various surface morphologies after the arc erosion process as caused by the break arc. We first investigated the morphology of the anode and cathode surface that was eroded by a single break arc. It is found that eight quite distinct types of the surface morphology are formed by repeated arcing. The formation mechanisms of the morphology types and the actions in arc erosion process can be explained
Keywords :
circuit-breaking arcs; electrical contacts; nickel alloys; silver alloys; wear; AgNi; CKS contact material machine; arc erosion process; breaking arc erosion; cathode surface; contact morphology; formation mechanisms; repeated arcing; surface morphologies; Anodes; Cathodes; Contact resistance; Force measurement; Machinery production industries; Materials testing; Scanning electron microscopy; Surface cracks; Surface morphology; Welding;
fLanguage :
English
Publisher :
ieee
Conference_Titel :
Electrical Contacts, 1993., Proceedings of the Thirty-Ninth IEEE Holm Conference on
Conference_Location :
Pittsburgh, PA
Print_ISBN :
0-7803-1270-8
Type :
conf
DOI :
10.1109/HOLM.1993.489665
Filename :
489665
Link To Document :
بازگشت