    Modified IEC 5000-h Multistress Aging of 28-kV Thermoplastic Elastomeric Insulators

  • Author

    Sundararajan, Raji ; Olave, Claudia ; Romero, Edwin ; Trepanier, Benoit

  • Author_Institution
    Electron. & Comput. Eng. Technol. Dept., Arizona State Univ. East, Mesa, AZ
  • Volume
    22
  • Issue
    2
  • fYear
    2007
  • fDate
    4/1/2007 12:00:00 AM
  • Firstpage
    1079
  • Lastpage
    1085
  • Abstract
    The 28-kV, novel, environmental-friendly, thermoplastic elastomeric insulators were tested under slightly modified IEC 1109 5000-h (Annex C) conditions for their long-term performance. The modifications were made to more closely represent the actual service environment than the conditions used in the IEC. Various stresses applied include UV-A radiation, heat, rain, clear mist and salt fog, in addition to electrical. After 5000-h aging, there was discoloration, loss of hydrophobicity, and a loss of hydrocarbon bonds. Overall, the insulators looked intact despite the molecular and microstructural changes
  • Keywords
    ageing; elastomers; insulators; 28 kV; IEC 1190 5000-h multistress aging; UV-A radiation; hydrocarbon bond loss; hydrophobicity; molecular-microstructural change; salt fog; thermoplastic elastomeric insulators; Aging; Contamination; Electric resistance; IEC standards; Plastic insulation; Polymers; Rain; Scanning electron microscopy; Thermal resistance; Thermal stresses; Accelerated aging; Fourier transform infrared spectroscopy (FTIR); equivalent salt deposit density (ESDD); hydrophobicity; multistress; scanning electron microscopy (SEM); thermoplastic elastomeric (TPE); thermoplastic elastomeric insulators;
  • fLanguage
    English
  • Journal_Title
    Power Delivery, IEEE Transactions on
  • Publisher
    ieee
  • ISSN
    0885-8977
  • Type

    jour

  • DOI
    10.1109/TPWRD.2007.893184
  • Filename
    4141171