    The suitability of a supermalloy thin film about 1 ¿m thick for use in 1 MHz power equipment was studied. The relationship between the hysteresis loss Wh and the maximum flux density Bm for the approximately 1 ¿m thick films deposited on SiO2 substrate is approximately Wh ¿ Bm1.75. This shows the same tendency as that for the rolled plate, where Wh ¿ Bm1.6, but the hysteresis loss value is one order of magnitude greater. In conventional rolled tape, the hysteresis loss is inversely proportional to tape thickness, but in the case of thin films, Wh obstructs any large-scale reduction in the loss.
  • Keywords
    Iron; Magnetic cores; Magnetic films; Magnetic flux; Magnetic hysteresis; Magnetic materials; Sputtering; Substrates; Thick films; Transistors;
  • fLanguage
    English
  • Journal_Title
    Magnetics in Japan, IEEE Translation Journal on
  • Publisher
    ieee
  • ISSN
    0882-4959
  • Type

    jour

  • DOI
    10.1109/TJMJ.1987.4549386
  • Filename
    4549386