DocumentCode :
955715
Title :
Influence of annealing temperature and time on hysteresis parameters and microstructure of an Fe/Co/V alloy
Author :
Pinnel, M. Robert ; Bennett, James E.
Author_Institution :
Bell Laboratories, Columbus, Ohio
Volume :
11
Issue :
3
fYear :
1975
fDate :
5/1/1975 12:00:00 AM
Firstpage :
901
Lastpage :
907
Abstract :
The variations in coercivity, remanence, and microstructure for 2frac{1}{2} hour aging anneals between 300°C and 1000°C on an Fe/Co/3% V alloy have been determined. Additionally, the effects of varying aging times for temperatures between 885°C and 925°C have been analyzed. Hysteresis parameters and optical microstructures were characterized on wire samples which had been either cold worked by stamping or remained undeformed prior to the aging anneals. Results show that the alloy exhibits maximum magnetic hardness in its initial cold worked or undeformed conditions. Aging anneals produce a general decrease in magnetic properties with increasing temperatures to 700°C. However, the deformed material exhibits a secondary maximum for aging temperatures between 590°C and 610°C. For anneals above 800°C magnetic parameters again increase as a two-phased, duplex BCC (α1+ α2) structure is developed. By varying the aging time for anneals that produce this duplex structure, a level of coercivity comparable to that achieved for a 600°C anneal was attainable. However, a comparable level of remanence and, thus, a similar squareness ratio, could not be produced with the duplex structures developed by aging near 900°C.
Keywords :
Hysteresis; Permanent magnet materials; Aging; Annealing; Cobalt alloys; Coercive force; Iron alloys; Magnetic analysis; Magnetic hysteresis; Microstructure; Remanence; Temperature;
fLanguage :
English
Journal_Title :
Magnetics, IEEE Transactions on
Publisher :
ieee
ISSN :
0018-9464
Type :
jour
DOI :
10.1109/TMAG.1975.1058770
Filename :
1058770
Link To Document :
بازگشت