  • Abstract
    The magnetic properties and the grain structure of 6.6Si.93.4Fe ribbons made by a rapid quenching roll method were measured after annealing the ribbons at about 1180°C for 60 minutes under pressures ranging from 5×10-1to 1.5×10-3Torr. By annealing the ribbon under the pressure of 3 × 10-1Torr the ribbon had highly oriented
  • Keywords
    Soft magnetic materials/devices; Annealing; Coercive force; Iron alloys; Magnetic flux; Magnetic materials; Magnetic properties; Magnetostatics; Magnetostriction; Silicon; Temperature;
  • fLanguage
    English
  • Journal_Title
    Magnetics, IEEE Transactions on
  • Publisher
    ieee
  • ISSN
    0018-9464
  • Type

    jour

  • DOI
    10.1109/TMAG.1981.1061696
  • Filename
    1061696