• DocumentCode
    989736
  • Title

    High flux density silicon-iron ribbons

  • Author

    Arai, K.I. ; Tsuya, N. ; Ohmori, K. ; Matsuoka, T. ; Shimanaka, H. ; Ohmori, Kenji ; Matsuoka, T. ; Shimanaka, H.

  • Author_Institution
    Tohoku University, Sendai, Japan.
  • Volume
    18
  • Issue
    6
  • fYear
    1982
  • fDate
    11/1/1982 12:00:00 AM
  • Firstpage
    1418
  • Lastpage
    1420
  • Abstract
    Silicon iron ribbons with silicon concentration lower than 4 wt% were prepared by a rapid quenching roll method, and the size of ribbons obtained were 2∼4 mm in width and 40∼60 μm in thickness. The grains grew to about 2 mm and the ribbons had
  • Keywords
    Annealing; Coercive force; Furnaces; Grain size; Iron alloys; Magnetic properties; Magnetostriction; Raw materials; Silicon alloys; Steel;
  • fLanguage
    English
  • Journal_Title
    Magnetics, IEEE Transactions on
  • Publisher
    ieee
  • ISSN
    0018-9464
  • Type

    jour

  • DOI
    10.1109/TMAG.1982.1061974
  • Filename